Hi Ed,
You do not say how large the LCCCs are nor on what substrate they are
mounted.
However, with this much Au in a vibratory environment one does not even have
to consider cyclic thermal expansion mismatches—these assemblies are in
trouble.
Some standard MIL vibration testing should give you a good indication and
convince management. That way you do not have to perform the more
resource-intensive thermal cycling.
The various Mantech studies (Martin-Marietta, early 1990's; etc.) should also
give you good information just on LCCCs on polymeric substrates.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|