TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 7 Apr 1999 10:47:09 EDT
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
"Stephen R. Gregory" <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
In a message dated 4/6/99 5:15:17 PM Pacific Daylight Time,
[log in to unmask] writes:

<< Dewey,

 I think within 2% fall out is ok for any chip shooter. I have worked with
 Mydata TP9-UFP & Fuji CP6 & this is good approximation  for chip component
 fallout.

 Ashok Tiwari
 SMT Engineer

 > ----------
 > From:         Access Control[SMTP:[log in to unmask]]
 > Reply To:     TechNet E-Mail Forum.;Access Control
 > Sent:         Tuesday, April 06, 1999 11:19 AM
 > To:   [log in to unmask]
 > Subject:      [TN] SMT Component Fall Out Rate
 >
 > Greetings,
 >
 > For all the SMT assemblers out there, what are your average fall out on
 > std. components, ie. 1206, 1210, 2010, sot-23, melf, minimelf.
 > I have 2 mydata machines and they run well under 2%. I wonder if 2% or
 > less than 2% fall-out is too high.
 >
 > Thanks in advance for any input.
 >
 > Dewey >>

Hi Dewey,

     I agree with Ashok, 2% ain't bad. Actually, when we quote supplying
attrition with the kits to our customers, I like to see 3%...but sometimes
the buyers who supply us material think they're doing a good job when they
give us exact quantities...1000 boards, 1000 parts....sheesh...
What really kills me is when they give us the 1000 parts in 100 piece
strips...fun stuff there...

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2