Hans,
I've had great success with the Struer's Accutom-50 Precision cut-off system. It can do both precision cutting (and you can program for example to "automatically" dice up a 225 I/O BGA into 15 rows of 1 ball wide each...) and/or do precision grinding where you "mill" down a surface a mil or less at a time. See http://www.struers.com/cutting.htm.
See
Jim
---------------------------------------------------------
Jim Maguire
Boeing Phantom Works
E/E M&P
Phone (253)657-9063
fax (253)657-8903
Pager (206)982-3737
email: [log in to unmask]
---------------------------------------------------------
> ----------
> From: Hinners, Hans - LYPME[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Hinners, Hans - LYPME
> Sent: Friday, April 30, 1999 5:18 AM
> To: [log in to unmask]
> Subject: [TN] Recommendations on a Versatile Microsectioning System?
>
> Hi Everybody,
>
> I was wondering if anybody could give me some leads on a versatile
> microsectioning system?
>
> I'm looking for a system which allows accurate microsections without needing
> to route the board or drill it for the registration pins.
>
> What's a reasonable accuracy? I don't really know *2 mils? *1 mil.
> Accuracy that doesn't add a zero to the price.
>
> Ideally, I need something that could do cross, z axis or angled sections.
> By z axis I mean similar to what they did for the Body Voyage CD-ROM (not to
> gross anybody out).
>
> Thanks,
>
> Hans
>
> Air Force Material Command - We keep them flying!
> ~~~~~~~~
> Hans M. Hinners WR-ALC/LYPME Bldg. 640
> Materials Engineer 380 Second Street,
> Suite 104
> Manufacturing Eng. Sec. Robins AFB GA 31098-1638
> 912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|