Hi,
Have anyone encountered that PCB from different suppliers give different
paste height.
We are using 3 PCB suppliers for one of our product, and the average paste
height we are getting (on 2 suppliers), using 6 mil stencil with rubber
squeegee (70 durometer) gives an average paste height of 6.5 mil. However,
there is one supplier's PCB that gives the average paste of 8 mil.
We need to double the squeegee pressure to achieve the paste height of near
7.0 mil
Could anyone advise me the cause to such issue.
Thanks
Poh
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|