Hi Kent - In terms of solderability requirements you could use
ANSIJ-STD-002A as your specification. Do you know what the metallization on
the resistors is? There are several different test methods within the
specification that can be used (Take a look and if you have additional
questions just shoot me an email). Good Luck.
Dave Hillman
JSTD-002A committee cochair
[log in to unmask]
"Kent S. Asmus" <[log in to unmask]> on 04/17/99 01:44:43 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Kent S. Asmus" <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] SMT Chip Resistors
All-
When sourcing precision thick-film SMT chip resistors with wrap-around
contacts, how does one typically control the quality of the delivered
product; i.e., contact solderability, contact integrity, etc? In other
words, what is the industry standard specification(s) that are typically
called out for such components? What is the appropriate IPC or EIA
standard?
I am also interested in finding out what tests can be conducted to
determine
the solderability of wrap-around contacts on SMT chip resistors.
I'm currently experiencing contact dewetting during reflow on about 20% of
the resistors obtained from a particular manufacturer. There also appears
to
be a significant number of chips with cracks in the wrap-around contacts.
Thanks in advance for any information you may be able to provide.
Regards,
Kent
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|