Dear team,
We have problem during dry film stripping, which is the process just before
etching.
During the dry film stripping, two stages of dry film stripping processes
are used and some of the Tin(act as etch resist) seems dissolve a bit at
the bare copper area just after stripping when in contact with stripping
solution of caustic soda and result etching problem. Especially for fine
spacing of 6-8mil, the incomplete etching problem are more serious and
sometimes re-etch the boards for twice again are required.
Do anyone have any idea to resolve it? The temperature employed is 40 C
and the conc. of NaOH is 150 g/L.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|