I don't know what happened to the first transmission, but mine came back blank.
If this is a duplication, just hit your delete key.
Regards,
Les
Hi Phil,
We looked at this possibility several years back. The main problem with
the conductive epoxies is that the electrical conductivity is too low for most
applications. With the ever increasing speed of many electronic devices and
needs, this even more compounds the problem. There is probably some nitch
markets where this technology may be feasable, such as the TOY market or some
other market that requires slow speeds and low current transfer.
.... Just my two cents worth...
Regards,
Les
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|