Hi Phil -
I haven't heard anything recently on this subject, but there was a major issue
probably fifteen or twenty years ago. In my recollection it involved some
U.S.Navy aircraft (possibly A-6 or F-4). If I remember correctly the
polyimide insulation of stranded wire bundles had been attacked and
deteriorated by some of the aircraft cleaning fluids. I'm not aware of any
fires, but it certainly was a situation that would have had the potential to
produce such.
I'm not aware of any prohibition of polyimide other than for wire jackets in
areas which may be exposed to certain strong alkalines.
How's about it? Anyone else out there got anything new or more accurate
recollections?
Note that Kapton is the DuPont registered trade name for their series of
polyimide materials. There are many other sources of polyimide products in
todays market.
Regards - Kelly
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|