Gary,
About 2 years ago, I had a product which had greater than 1000
components (0603) on the underside.
No issue
The underside was printed using a 0.010" stencil and Locitite 3607.
The aperture size was an oblong shape , 0.030" long x 0.015" wide.
A minimum of 0.010" gap between the aperture and pad, both sides.
The 0603 pad was 0.043" x 0.026".
Hopes this helps you