Good Morning TechNet,
I have a fabrication drawing with a note with the following note.
Material: .062 laminated glass (woven fabric) base, epoxy resin, Flame
retardent, FR4.
copper clad 2 oz./sq ft. Laminate must be certified to
have a minimum comparative
tracking index of 175. Microsection demonstrating
compliance with copper weight,
dielectric spacing, line width and use of CTI 175 or
better material shall be shipped
with each lot.
I am at a loss on the CTI 175 stuff. I have reviewed IPC 4101 and don't
find a reference. I have
placed a call to our material supplier but no response yet. The TechNet
seems much faster.
Can anyone provide me with a clue? Thanks in advance for the help.
Anne Ledger
EMDS, Inc.
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|