Anyone out there doing intrusive reflow with OSP mixed tech. (SM + TH) double
sided boards? We are considering it (for cost and cycle time purposes). Do you
get good solder filets for the TH parts (knowing that you have decreased wetting
action in OSP holes vs. HASL)? Any other issues to be aware of?