What range of SIR can be reasonably expected on PWBs made from epoxy
glass and polyimide glass materials? Bare board and post assembly.
Assembly is manual using both through-hole and SMT parts, using rosin
flux. Cleaning is done either in a vapor degreaser (using an n-propyl
bromide solvent) or by cold washing in isopropyl alcohol. Thanks.
--
Bob Felton
[Micro Instrument Co., Escondido, CA]
([log in to unmask])
################################################################