Richard,
This time, I guess, your design engineering manager is right. There is a fluxless soldering process available. If I remember correctly, one process I am aware is called *PADS* (Plasma Assisted Dry Soldering???). Wow... a fancy jargon isn*t it? In this process, components or assembled boards are exposed in a PADS treatment within a vacuum chamber. This treatment turns soldering surface to oxide-resistant by modifying soldering surface layer. From there, you can store components or assembled boards for a specified period prior to wavesoldering, reflow or handsoldering. You don*t need to apply flux to allow wetting, thus no cleaning is required.
This process is ok for a lab application or a small production run. I don*t have the info handy, but I am sure I have it filed away in my filing cabinets. I can dig out something for you if you need to look further.
Regards
Matthew
Norsat International Inc.
>>> Richard Hamilton <[log in to unmask]> March 10, 1999 8:46 am >>>
Hello fellow TechNetters,
Well, we were asked a question by the design engineering manager yesterday
if we had considered a fluxless soldering process. We are aware of a process
called Solid Solder Deposit (SSD), but not a fluxless process by name.
After the manager read us the email he got from one of the marketing types,
I tend to believe that he was referring to no-clean process because of a
reference in his note about cleaning boards at a previous manufacturer (TI).
My guess (oh how I hate to guess/assume) is that this marketing type has
just mixed up a couple of buzz-words together,.....kinda like 'military
intelligence'. I mean look at it, 'no-clean flux', I can see how a sales
person would want to shorten that to 'no-flux'. Now as usual, it is up to us
manufacturing people to invent the process that has been sold to the
customer!!
And as a side note: Steve -
Your comments on machine maintenance are RIGHT ON!! You couldn't be more
correct. Sometimes I cringe at the way some machines are treated, and the
surprise that goes on when it does drop out!
Thanks all.
Richard Hamilton
Clemar Mfg. / Rain Bird
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|