When referring to IPC-SM-840, it is very important to remember that this is a
material qualification document only, with all the test requirements applicable only
to a defined test coupon--not to production boards. Jack
==========================================
APEX - the industry's premier trade show in Electronics
Manufacturing, March 12-16, 2000, Long Beach, California.
More information on website www.ipc.org/html/apex.htm
-----------
Jack Crawford, IPC Director of Assembly Standards and Technology
2215 Sanders Road, Northbrook IL 60062-6135
[log in to unmask]
847-790-5393
fax 847-509-9798
>>> KELLY M SCHRIVER <[log in to unmask]> 03/30/99 12:15PM >>>
Hi Kelly -
May I direct your attention to an interesting little requirement out of
IPC-SM-840C? A portion of para. 3.4.10 reads: "The board fabricator shall
confirm that the minimum thickness is sufficient to withstand 500 VDC per
solder mask vendor's specification. The coating thickness shall be measured
by any micrometer or inidcator accurate to 0.0025 mm [0.0001 inch] or
microsection in accordance with TM 2.1.1 of IPC-TM-650."
"If a specific thickness or breakdown voltage is required it shall be
specified by the end user on the procurement document."
Thickness of the solder mask is considered critical only in an electrical
performance sense. There is no relief for any areas which are to be coated
with permanent solder mask on the circuit board from this requirement.
Regards - Kelly
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|