KELLY M SCHRIVER <[log in to unmask]>
Date:
Mon, 22 Mar 1999 08:43:00 -0500
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, KELLY M SCHRIVER <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
Good morning Ken -

Recommend you contact Michael Crutchfield at DuPont in Research Triangle Pk.,
NC - (919)248-5010.

Their Pyralux AP material gets away from the age old problem of having an
acrylic adhesive with a Tg of ~40C in the midst of an otherwise high
temperature laminate structure.  As an assembler, we have seen our in process
problems, such as delaminations and "white spots" eliminated.  Our suppliers
also report improved fab yields.

Regards - Kelly

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2