I would worry more about the "replacement"/"repairs"/"reworks" than leaving
it as is ;
Have to agree with Steve ; no need to push 603 pads needlessly .
Sorry to disagree Matt ; but I'd prefer to drive without sus reworks .
Secondary validation :
STELLA ; to be able to sleep without nightmares of freeway pile ups :
Find yourself a relevant quick test ( accelerated cycling ) some you can
close in week ,
if Werner won't pull one out of his hat I'll dig in my files ; but it's
really his hobby .
With 805's you should have no issues ; but you'll have to validate it :
Primary validation :
Perhaps the fastest rubber stamp in your sector :
Get it through relevant (standards set you work to) vibrating test ; the
cycling considering it's battle of two small passives and less load on 805's
anyhow would be perhaps useless delay as well (do it as a follow up)
Pull or shear tests are not relevant in this dimensions ; as vibro test
should indicate .
See you Stella
Paul Klasek
http://www.resmed.com
PS
the expert really is Werner (although he proved to be mortal on rare
occasions too) ; I took the liberty (as usual) to list him on send ;
hopefully he'll bite with specifics, correctly worded reflecting worsening
legal climate nowadays .
> ----------
> From: Matthew Park[SMTP:[log in to unmask]]
> Sent: Tuesday, 2 March 1999 6:50
> To: [log in to unmask]
> Subject: Re: [TN] Soldering fillet
>
> Stella.
>
> I know this sounds silly. Replace 805 pkg resistors with 605 pkg
> resistors. Believe me it is a wiser option than fiddling with pull
> test, vibration test, reliability test....so on.
> Anyway, Who is your end-customer, GM, Chrsyler, Ford, Nissan
> or Toyota? Hey, making sure my next car won't crash on me
> with repair bills...
>
> Matthew
> Norsat International Inc.
>
> >>> <[log in to unmask]> March 1, 1999 7:56 am >>>
> Dear experts,
> We are building electronics for automotive industry.
> We have a number of boards where 0805 package resistors
> were placed and
> reflowed on the 0603 pads. As the results there is no side
> concave solder
> fillet, only under the component terminations.
>
> What options other than scrapping the boards would you
> suggest? ( Rework:
> remove and replace. Do some testing (vibration, pull test??).
> Please, help
> Thank you, very much
> Stella N
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using
> LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to
> [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at
> [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|