Address,
We have an application where we are using OA Flux and Paste to process
RF PCMCIAs. The PCAs are thoroughly cleaned prior to test. I'm still
having test issues with RF PCMCIAs.
If I remember correctly, I read an article that discussed cleanliness of
PCAs that are RF. If the PCA is not thoroughly cleaned, the organics
will wreak havoc on the RF tests. There are chemistries (saponifers)
available that will reliable remove the excess organics and provide
enough cleanliness to pass RF testing.
CAN someone please provide some more light onto this issue or give me a
direction to pursue, e.g., contacts. Thanks.