John,
I assume you want to use these for some sort of through-hole
reflow application, like pin header soldering. Many solder preform
vendors make doughnuts held together with a very small solder rib
between the doughnuts that separates during reflow. This eliminates the
kapton requirements and additional costs/handling.
Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX 77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]
> -----Original Message-----
> From: Arroyave, John (FL51) [SMTP:[log in to unmask]]
> Sent: Wednesday, March 03, 1999 8:40 AM
> To: [log in to unmask]
> Subject: [TN] Any Info on Solder Preforms with 0.100" centers
> held together by Kapton?
>
> Does anyone know of a manufacturer or vendor that may make or sell
> this
> product, if it exists? We are basically looking for individual
> preform
> "doughnuts" that are held in place by Kapton or some other similar
> material,
> that can be removed after re-flow. I looked into Winslow Automation's
> SolderQuick product, but apparently they only do re-balling for BGAs
> on
> Kapton like material. Any information would be greatly appreciated.
>
> Thanks,
>
> John Arroyave
> SMT Production Engineer
> Honeywell Space Systems
> Phone: (727) 539-2272
> Fax: (727) 539-4469
> e-mail: [log in to unmask]
> <mailto:[log in to unmask]>
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|