TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Francis Lai <[log in to unmask]>
Date:
Wed, 31 Mar 1999 18:01:47 -0800
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
Parts/Attachments:
text/plain (19 lines)
I used current density 15mA/cm**2 in our Macdermid tin-lead bath for 5
min. and I got 110 uin. with a 67% tin. But when I change the current
densities to 7.5mA/cm**2, I got 140 uin. with a 75% of tinfor 10 min..
My question is will a change in current densities in a Macdermid
tin-lead bath screw up the composition of Tin and Lead?
My e-mail : [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2