TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Jim Kittel <[log in to unmask]>
Date:
Wed, 31 Mar 1999 15:31:26 -0700
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (173 lines)
Bev,
The problem I encountered was during removal/replacement of the
component.  At that point the gold had already dissolved into the
tin/lead paste during initial soldering.   The metal remaining on the
pad was the nickel and it was not solderable.  The abrasion I did was on
the nickel oxide in preparation for re-attaching the new component.

Jim Kittel

>-----Original Message-----
>From:  Bev Christian [SMTP:[log in to unmask]]
>Sent:  Wednesday, March 31, 1999 1:12 PM
>To:    [log in to unmask]
>Subject:       Re: [TN] Ni/Au "black pad" problem
>
>Jim,
>If we are talking about a problem that is occurring at the gold/nickel
>interface I do not understand how cleaning the top surface of the gold with
>an eraser is going to help you soldering.  Please explain.
>
>regards,
>Bev Christian
>Nortel Networks
>
>PS Yes, we are experiencing this problem.  Rarely, but when it happens it is
>a BIG mess.
>
>> -----Original Message-----
>> From: Jim Kittel [SMTP:[log in to unmask]]
>> Sent: Wednesday, March 31, 1999 8:50 AM
>> To:   [log in to unmask]
>> Subject:      Re: [TN] Ni/Au "black pad" problem
>>
>> Janice,
>>
>> I also recently experienced a pad situation similar to what you
>> described on a 10 layer nickel/gold immersion PWB surface.  We assembled
>> a prototype board for engineering using RMA paste and an
>> aqueous/saponifier cleaning process.  The board contained two 432 pin
>> BGA's, one of  which I had to replace for electrical reasons (lab power
>> supply voltages had been reversed).  I used an Airvac hot nitrogen gas
>> system to remove the BGA.  Upon removal, 90% of the pads were completely
>> stripped of solder and would not wet with an iron.  They appeared dark
>> and looked like passivated nickel.
>>
>> I showed these pads to our fab PWB vendor.  He wanted to do some
>> checking on his nickel tanks, but thought the gold may have been too
>> thin, allowing passivation of the nickel under the gold, prior to
>> assembly.
>>
>> In reworking the pads I tried a 10% solution of HCL, which didn't help
>> solderability.  I finally resorted to using an erasure to polish
>> (abraid) the pads.  Solder iron testing proved the pads readily accepted
>> solder.  I then screened an aggressive water soluble paste on them and
>> reattached a new BGA.  The process was successful.
>>
>> Some day I hope to retrieve this board from engineering and remove the
>> second BGA.  Hopefully this pattern will exhibit the same phenomena and
>> I can do some cross sections and more detailed analysis.  I am concerned
>> as you are about long term reliability, and need to understand this
>> situation better.
>>
>> Maybe other readers will share their experiences.
>>
>> Jim Kittel
>>
>> >-----Original Message-----
>> >From:  Janice M. Pelchat [SMTP:[log in to unmask]]
>> >Sent:  Tuesday, March 30, 1999 5:11 AM
>> >To:    [log in to unmask]
>> >Subject:       [TN] Ni/Au "black pad" problem
>> >
>> >We are looking for experiences with a problem that apparently manifests
>> >during the immersion nickel/gold process.
>> >
>> >As I understand it (pardon lack of technical expertise) the narrower fine
>> >pitch pads have less nickel surface than larger pads and during the
>> >nickel/gold exchange, there is some chemical process that results in
>> >entrapment between the remaining nickel and gold surface.
>> >
>> >This is not visible to the naked eye.  It survives the "tape test" at
>> >incoming inspection, it is not lot specific, it does not manifest as
>> >"blackened pads" until being exposed to the flux/reflow/cleaning process.
>> >
>> >These pads are "reworkable", but the rework requires component removal,
>> >slight abrasion, "retinning" of the pad, etc.
>> >
>> >We have seen this across our PWB supplier base (providing the Ni/Au
>> >immersion boards).  It is apparently inherent in the chemistries involved
>> in
>> >the process.
>> >
>> >This is a relatively new problem for us.  Does anyone out there have any
>> >long term experience with this?  What about reliability issues?  Latent
>> >failures?  Have you determined when a board should be reworked or
>> scrapped?
>> >
>> >
>> >Our major issue is that we cannot get recovery from some suppliers when
>> this
>> >problem manifests.  Retooling charges for various boards is prohibitive.
>> We
>> >are exploring OSP as an alternative.
>> >
>> >Janice M. Pelchat
>> >SR Quality Engineer
>> >Benchmark Electronics
>> >Hudson Division
>> >
>> >Email:  [log in to unmask]
>> >Voice:  603-879-7000 ext 2412
>> >Fax:     603-879-7157
>> >
>> >################################################################
>> >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
>> 1.8c
>> >################################################################
>> >To subscribe/unsubscribe, send a message to [log in to unmask] with
>> following
>> >text in the body:
>> >To subscribe:   SUBSCRIBE TechNet <your full name>
>> >To unsubscribe:   SIGNOFF TechNet
>> >################################################################
>> >Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>> section
>> >for additional information.
>> >For technical support contact Hugo Scaramuzza at [log in to unmask] or
>> >847-509-9700 ext.312
>> >################################################################
>> >
>>
>> ################################################################
>> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>> ################################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
>> following text in the body:
>> To subscribe:   SUBSCRIBE TechNet <your full name>
>> To unsubscribe:   SIGNOFF TechNet
>> ################################################################
>> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>> section for additional information.
>> For technical support contact Hugo Scaramuzza at [log in to unmask] or
>> 847-509-9700 ext.312
>> ################################################################
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2