The FR stands for Fire Resistant, and the 4 is part of the NEMA designation.
IPC 4101 has a wonderfully tabulated breakdown of each of these base
materials.
The specification sheets do not indicate (to me at least) a correlation
between the number, like FR-2, FR-3, or FR-4 and any of the physical
properties, but this is a guess. I think it has more to do with which came
first, as the FR-1 is a "Phenolic, Flame Resistant", FR-2 is a "Modified
Phenolic, Flame Resistant" and FR-4's are all epoxy and vary by MIL spec.
Hope this helps, and I would love to know if there is a physical reason for
the numbering system.
Jonathan Meigs
Product Development
Oak-Mitsui
-----Original Message-----
From: Jim Marsico 516-595-5879 [mailto:[log in to unmask]]
Sent: Monday, March 29, 1999 1:56 PM
To: [log in to unmask]
Subject: [TN] LAMINATE DESIGNATION
Can anyone tell me what the F,R and 4 means for FR-4 material?
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|