Hi, Guenter, Werner...
An opinion within the group of "leading lights" of UK technology,
claim that "the lead free legislation is good timing" as Sn/Pb alloys
do not have the reliability of other alloys, particularly with regard
to modern components such as CSPs and Micro BGA.
I have always understood that Pb makes Sn/Pb alloys very plastic and
thus extreemly reliable under the stresses of thermal cycling.
If there are more reliable alloys, what might they be?
Which alloys present us with a higher degree of plasticity?
Regards
Edward Brunker
PSION Computers
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|