Sender: |
|
X-To: |
|
Date: |
Fri, 26 Mar 1999 12:47:57 -0600 |
Reply-To: |
|
Subject: |
|
From: |
|
In-Reply-To: |
|
Content-Type: |
Multipart/Mixed;
boundary="BeyondBoundary_12_Fri_Mar_26_12:47:58_1999__6DF1" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Hi Kelly,
Hey!, I want to know what the age is for Geezerhood. Apparently you and
I are still working although I'm finally going to hang it up this month. Feel
like I may have attained the age of Geezerhood myself, hehehe!! May keep my
consulting shingle out, should someone have the audacity to hire me. It may be
Feast or Famine out there. I'll miss all the commaradie of the technetters I'm
sure. Should I be so fortunate to find some support for my consulting, maybe
I'll see you folks at IPC.
See Ya !
Les
> From: KELLY M SCHRIVER <[log in to unmask]>, on 3/25/99 3:02
> PM:
> Hey Graham -
>
> Thanks for the addition - like you, I'm a little leery of what the "expert"
> said, or at least the words used in the media to describe what they thought
> he
> said. Not that this could not have occurred, but it sounds like and awful
> lot
> of supposition, with no indication that supports established fact.
>
> In my recollection, the U.S. military "limited usage" rather than "banned
> usage". There is, and has been for many years, a limitation on PTFE
> jacketed
> wire as a result of its cold flow charactaristics.
>
> Guess I've gotten somewhat skeptical since I've grown into geezerhood.
>
> Y'all have a fun day - Kelly
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
|
|
|