We have a CyberSentry automatic paste inspection system for our SMT lines. I am
trying to establish warning & failure limits for each of our boards.
I would like to know if anyone has any recommendations in percentage of the
paste height, volume, and area for limits they set. The engineer said he has
used 20% for the warning limits. ( i.e. on a 6 mil stencil, 6.5 mils nominal +/-
1.3 mils (20%) )
Does this sound like a fair number?
I would like to get a feel for what other manufacturers are using for their
limits.
Thanks in advance,
Rob Watson
Sanmina Corp.
Plant 10
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|