Why does hot DI water etch solder?
We have a water wash process for our avionics cards and we sometimes find
that the idents have been removed from some of the components. Could this be
due to the hot DI water?
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
11/03/99 00:18
>From: Russ
>Sent: Wednesday, March 10, 1999 4:02 PM
>To: 'Manish'
>Subject: RE: [TN] Dull Solder Bump
>
>
>Hello Manish,
>Guess what? The cleaner your DI water the worse the problem. Get some
>hot, very pure DI water and just try a quick test. The DI water will
>etch away the solder until you have no bump left.
>
>Also watch out for flux left on the wafer after reflow. Most water
>soluble fluxes are organic acid based and can still have some pretty
>good activity left in them even after reflow.
>
>Fast cooling, no vibration, cool DI water spray rinse (without
>recirculation), Hot clean DI (short time only) should have your bumps
>shinning pretty. Of course most of this is purely cosmetic.
>Solderability shouldn't be impacted by by the dull solder appearance.
>
>Regards, Russ Winslow
>
>Six Sigma
>1940 Concourse Drive
>San Jose, CA 95131
>
>[log in to unmask]
>http://www.sixsigmaservices.com
>
>
>
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Manish
>Sent: Wednesday, March 10, 1999 2:58 PM
>To: [log in to unmask]
>Subject: [TN] Dull Solder Bump
>
>
>Hello Everyone:
>
>I am trying to design am experiment to study the surface appearance of
>solder bumps and its effect on the shininess/dullness of bumps. One of
>our customers recently reported an increased rejection rates at their
>placement machine as the dull solder bumps were not recognized.
>
>Although we have not conducted extensive experiments in house to study
>the
>effect of reflow profile, cooling rate and the flow of nitrogen etc., i
>would appreciate feedbacks regarding your experience with this issue.
>
>We also rinse our wafer lots with DI water after reflow. Is there a
>possibility of impurities in DI water attacking the surface of eutectic
>solder. All of the wafers we bump are near eutectic solder alloy
>composition. The issue of dull solder bumps seems to be a periodic
>issue,not surfacing regularly.
>
>I would appreciate your comments on factors responsible for causing dull
>bumps.
>
>Regards
>Manish
>
>PS I am only refering to the occurence of dull solder bumps after wafer
>reflow. We use a water soluble flux during the wafer reflow.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
>1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
Mark Austin (Process Engineer)
ACW Technology Limited
Hylton Road
Petersfield
GU32 3XX
ENGLAND
TEL - +44 (0) 1730 300000
FAX - +44 (0) 1730 266045
Email - [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|