TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Tue, 9 Mar 1999 15:11:10 -0600
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (34 lines)
From: Dennis J Fall@TFT on 03/09/99 03:11 PM


To:   [log in to unmask]
cc:
Subject:  Etchant for Copper Assuming Sn/Pb Resist

Where (if anywhere) can I get an etching chemistry that will remove
approximately 1000-3000 angstroms of copper, but will not harm
electroplated Sn/Pb?  If possible, I would also like to remove 1000-3000
angstroms of Nickel-Chromium that is under the copper at the same time I
remove the copper.  I will greatly appreciate any help.


Thank You

Dennis Fall                        P: 507-625-8445 x17

Engineer                           F: 507-625-3523

Thin Film Technology Corporation

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2