John,
You've typed negative comments regarding Omikron Immersion Tin on Technet
before. I send you my number, my address, I e-mail you to try and help, and
you refuse to contact me. I'm starting to wonder if you couldn't care less.
You are misinformed about the deposit thickness of Omikron, it will deposit
40+ microns no problem.
I'm not going to bother asking you how you got the information, who ran
the tin, how you measured it, etc. on Technet. If you're serious about
getting some good documented information on the Omikron please contact me. I
will connect you with our Ph.D. chemists and the formulator of our Omikron
Tin, which by the way, is every bit as good as Dexcoat if not better.
By the way John, we also sell a fair amount of solder paste and assembly
products nation wide, Canada, and a few other places, something I believe
Dexter does not deal with. This gives us strength in technical support for
issues just like the one you have right now in assembly. Give us a call.
Stephen M. Wentz
Florida CirTech
(408)233-0443
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|