It's GFN. Mil-P-13949/4 or the new IPC-4101/2. The BMS I can't even
guess at.
Larry Campbell
BFGoodrich, Avionics Systems
>>> Mike Zagami <[log in to unmask]> 02/12/99
03:45pm >>>
I have a spec that call for the following material:
.062 flame retardent glass epoxy board, copper-clad on one or two
sides as required. Mil-P-13949, type 6FN (or BMS 8-120, Type 1, class 4,
Grade A)
I cannot find info on the "6FN" material. The closest I could find
was "GFN". Is there such a material as 6FN. And also what is the "BMS"
spec?
Thanks,
--
Michael Zagami
Electrical Engineer
Fairchild Controls Corp.
301-228-3469 (voice)
301-682-6885 (fax)
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|