Angie Margues,

Contact Scott Gordon of  Electronix, Carson City. Nevada.
Tel: 702-782-2545.  He is a Panasonic used broker, and he will
get you whatever  you are looking for.  Don't forget to  mention my
name to him.  I wanna get cheap prices all Panasonic spares
and junks that I will be needing from him next time.

regards
Matthew Park
Norsat International Inc.

>>> Angie Marques <[log in to unmask]> February
9, 1999  2:57 pm >>>
I am looking for a AC Servo Amplifier (circuit board) for a
Panasonic
Pick-n-Place machine. This card can be used on the MV100 or
MPA 80. Does
anyone know where I can purchase or repair the one I have with
minimum
lead time? Panasonic gave me a 8 week lead time.

Angie Marques
SR Process Engineer
Quadrus Manufacturing
408-918-5045

################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line
Services" section for additional information.
For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2