Vickie -
A picture is worth 1k words. Why not grab your sections and bring them over
to our lab for a second opinion. We're in your neighborhood, across from NH
Tech in Nashua; just give us a call.
Cheers!
Bob Lazzara
Circuit Connect Tech Support
TEL: 800.560.9457 FAX: 888.453.0520 BBS: 603.889.5385
alternate eMail: [log in to unmask]
-----Original Message-----
From: Vickie Dycewicz <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Tuesday, February 02, 1999 1:02 PM
Subject: [TN] Removing Debris from Holes before Electroless Deposition
>I am looking for information on what companies are using to remove debris
in
>holes before the electroless deposition (dep) process.
>
>We are getting pth voids in holes due to drill debris still in the holes
after
>deburr, before dep. Cross section pictures of the pth void show a
circumfrential
>void, near the center of the hole. The electroless copper leading up to the
void
>is very granular, as if trying to dep over debris. I do not classify them
as
>bubble voids because of the debris still left in the hole.
>I predominately see these voids in 0.022 holes, 0.261 panel thickness.
>After drill the panels are hand sanded, then through our deburr process
which is
>an IS Scrubbex with 350psi high pressure spray section.
>
>I would greatly appreciate any suggestions on how to improve my process.
>
>Thanks,
>Vickie Dycewicz
>Electroless Deposition Process Engineer
>Teradyne, Inc.
>Nashua, NH
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|