TECHNET Archives

February 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Tenison Stone <[log in to unmask]>
Date:
Thu, 25 Feb 1999 07:03:20 -0600
Content-type:
text/plain; charset=us-ascii
X-To:
Alain Mathieu <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (74 lines)
Alain,

Check with intermec.  They should have all the information including UL and
CSA specifications.  I check out all of this information when I choose a
label.  Not all labels are UL or CSA approved.

Tenison Stone
Telex Communications




Alain Mathieu <[log in to unmask]> on 02/23/99 09:38:06 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Alain Mathieu <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Tenison Stone/BlueEarth/Telex)
Subject:  [TN] Labels on product for outside use




Hi TechNetters!

We are using InterMEc labels on our products. Labels material is
polyester film with acrylic glue. We are using Intermec ribbon too.

Recently one big custommer has asked us to give them a warranty on those
lables.

Here is my questions: Is anybody out there using intermec labels and
ribbons for product that are installed outside and in any region from
south America to up North where it is presently -30oF   and to what king
of life expectancy we might figure out.

Lables are glue to epoxy paint over aluminum. product is specified for
-40 to +150oF.

We have started a few months ago only to use those labels.

Alain Mathieu
Electroline Equipment Inc.
(514) 374-6335
(fax: (514) 374-6948
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2