Do not know if it is an ANSI document but AMS 2422D is an Aerospace Material
Specification published by the SAE The Engineering Society for Advancing
Mobility Land Sea Air and Space It covers the engineering requirements for
electrodeposition of Gold and the properties of the deposit. The SAE may be
reached at http://www.sae.org
> -----Original Message-----
> From: Michael D. Doty [SMTP:[log in to unmask]]
> Sent: Wednesday, February 17, 1999 2:30 PM
> To: [log in to unmask]
> Subject: [TN] Gold spec.
>
> Hi Techies,
> I'm looking for info on the following spec. ANSI/AMS
> 2422C.
> I believe this a gold spec for electronic applications.
> Thanks in advance for the help.
>
> Mike Doty
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|