Hi Russ,
Well, your problem comes down to two possible causes:
1) no solderability; your tests seem to exclude that.
2) inadequate soldering process; it certainly is possible that the solder
balls were never properly attached to the component. Your problem is not
likely related to shear strength of (or crack propagation in) nickel-tin
intermetalics, but the absenceof any IMCs which are the by-product of a good
intermetallic bond resulting from good wetting. Solder attachment strength to
nickel is about half that to copper.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|