Hi Howard - this is probably an overkill answer to your question but since
you asked:
Oxygen free copper (OFHC - oxygen free high conductivity) is a copper alloy
that is produced by remelting electrorefined cathode copper (ETP) and
casting it under a reducing atmosphere of carbon monoxide and nitrogen so
that oxygen does not enter the copper and form a Cu2O phase. The Cu2O phase
(which is present in ETP copper) reduces a copper alloy's electrical
conductivity. OFHC copper is preferred for many electronic applications
because of this improved electrical conductivity. Also, OFHC copper is
typically free of gas porosity and hydrogen embrittlement problems that can
be found in ETP copper. But - OFHC copper is more expensive than ETP copper
due to the additional processing required to produce the alloy! Hope that
helps.
Dave Hillman
Rockwell Collins
[log in to unmask]
Howard Lin <[log in to unmask]> on 02/09/99 10:47:38 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
To: [log in to unmask]
cc:
Subject: [TN]
$B2sJ$ (B : [TN] Looking for OFHC copper and cleaner
What does it mean ""Oxygen Free High Conductivity (OFHC)" copper ?
Howard
> -----
$B86;OM97o (B-----
> $B4s7o<T (B: [log in to unmask]
> [SMTP:[log in to unmask]]
> $BQ#Aw;~4V (B: 1999 $BG/ (B2 $B7n (B3 $BF| (B PM 11:18
> $BZ@7o<T (B: [log in to unmask]
> $B<g;] (B: [TN] Looking for OFHC copper and cleaner
>
> My company is located in El Paso, and I cannot find any local lab
> supply stores
> that have "Oxygen Free High Conductivity (OFHC)" copper (75 mm X 25 MM
> X 1 MM).
> Does anybody know who supplies these coupons? Also, I am trying to
> find some
> liquid copper cleaner. Your assistance would be appreciated.
>
> -Thank you,
>
> Teo Tijerina
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
|
|
|