David Muscat wrote:
>
> Ed
> You must have been in some strange frame of mind whilst reading our reply to Nick. What sort of cookies do
> you eat ? Obviously not the same as our Anzac Cookies! We certainly didn't imply we were going to charge
> for the Information.
David,
I suspect Ed's reaction comes from the sheer size of your
ad material; even as a North American resource for many
of the same points I took your message the same way.
In most 'net forums and newsgroups, 4-line "signatures"
are taken as non-offensive. Going beyond that tends to
draw flames or worse, dismissal of content or entry in
filters.
OTOH, if you've accomplished reliable wave soldering of
.8mm gull-wings my hat is off to you, sir.
Regards,
--
Jeff Seeger Applied CAD Knowledge Inc
Chief Technical Officer Tyngsboro, MA 01879
jseeger "at" appliedcad "dot" com 978 649 9800
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|