Alon
I agree preheat is critical to all wave solder operations. Flux
selection and pretinning of component leads where possible will assist
in using lower preheat temperatures.
I have visited a company in Chicago which makes custom Mini-wave
machines.
Contact: New Age Electronic Devices Inc. at 773-973-3296 ask for John
Susco. Please tell him we spoke. Call me at 603-896-2151 if I can be
of further help. Leave a message and I will call back.
Regards
Ken Morrison
Sr. Process Engineer for Through Hole assembly of backplanes
HADCO VAM East
______________________________ Reply Separator _________________________________
Subject: Re: [TN] Wave soldering machine
Author: Ryan Jennens <[log in to unmask]> at SMTPLink-Hadco
Date: 2/9/99 5:42 PM
Alon-
When I first started working at the company I am at now, we had what you
call a "bench top" wave solder machine. It was only about 4' long, used two
carriers to transport the boards, had 1' of pre-heat, and had about 200 lbs.
of solder in the pot. The problems we had, although we got good solder
joints using water soluable flux, was that the one foot of pre-heat was
nowhere close to enough pre-heat to get the board up to temperature. We had
the preheats at 100% and we would blast each cap on the board. I can
garauntee we were not following the recommended profile. If I were you I
would be weary of "bench top" wave solder units. If you find one that sits
atop a bench, be sure it has enough pre-heat to ramp the board at an
appropriate rate.
Ryan Jennens
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Alon Beitner
> Sent: Monday, February 08, 1999 2:46 PM
> To: [log in to unmask]
> Subject: [TN] Wave soldering machine
>
>
> I am thinking of buying a small bench-top wave soldering machine to do
> some small run
> prototype soldering. My components are all through hole and are
> standard so the
> machine can be very simple. Can you suggest which machine I should look
> at and how I
> may find a used one. Thanks.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask]
> or 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|