Would it be so severe in normal ambient cycle Werner ?
Even 90'C span over 24 hours seems (likely mistakenly?) pretty mild ?
I came across this as well ;
is there any average daily span ? in say average Alaskan warehouse ?
Could you elaborate a bit also on that 20'C cross line significance I noted
in the 785 standard ?
Could it be said storage forms equal part of the product life & warranty
considerations ?
Thanks ahead
Paul Klasek
http://www.resmed.com.
> ----------
> From: Werner Engelmaier[SMTP:[log in to unmask]]
> Sent: Friday, 5 February 1999 7:47
> To: [log in to unmask]
> Subject: Re: [TN] Storage of assembled boards at - 50 degrees Celcius
>
> Hi Daan,
> Your problem is not storage at -50C, but storage from -50C going up to
> maybe
> +40C and back down again. That is a rather severe thermal cycle, which if
> repeated too often may cause failures, especially of solder joints.
>
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL 32174 USA
> Phone: 904-437-8747, Fax: 904-437-8737
> E-mail: [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|