Steve,  The only company I know of that sells brush plating solutions is Sifco Selective Plating in Cleveland.  However a search through the Thomas Register also turned up a place call Brushtek in Chatsworth, CA.  Good luck!

Sheila Smith, Marconi AES 

----------
From:  Leslie O. Connally
Sent:  Wednesday, January 20, 1999 9:48 AM
To:  [log in to unmask]
Subject:  Re: [TN] Assy: Source for Gold Plating Solution

Hi Steve,

        You might try Technic, Inc. Their California rep's address is:

        Technic, Inc.
        1170 Hawk Cir.
        Anaheim, Ca. 92807
        (714)632-0200
They also have a web site at www.technic.com

Another source is Lea-Ronal. The only address I have is a New York address, but
I'm sure they must have a West coast rep. Their address is:

        Lea Ronal
        272 Buffalo Avenue
        Freeport, N.Y. 11520
        (516)868-8800

Their President is Richard Kessler.
>  From: "Stephen R. Gregory" <[log in to unmask]>, on 1/19/99 1:57 PM:
>  Hello out there!
>
>       Remember my post last week about solder preforms for PC104 connectors?
>  Remember what I was whining about? 'Bout the difficulty in hand soldering
>  those things without getting solder on the gold plating?
>
>       Well, you can guess what this email is about...I need some gold plating
>  solution now. (BIG surprise there huh?)
>
>       The source I used to get it from here in "Silicon Valley" has
>  disappeared...does anybody know of another source I can buy it from? It
>  would
>  be kinda' nice if it was here in the valley, but not nessesary.
>
>  I'd sure appreciate it!
>
>  -Steve Gregory-
>
>  ################################################################
>  TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>  ################################################################
>  To subscribe/unsubscribe, send a message to [log in to unmask] with following
>  text in the body:
>  To subscribe:   SUBSCRIBE TechNet <your full name>
>  To unsubscribe:   SIGNOFF TechNet
>  ################################################################
>  Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>  for additional information.
>  For technical support contact Hugo Scaramuzza at [log in to unmask] or
>  847-509-9700 ext.312
>  ################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2