Frank and Earl,
Don't forget that if you must place construction characteristics such as line
widths, and thicknesses on the drawing, make them for reference. The primary
concern is that the impedance of the transmission line falls within the stated
tolerance, not the individual features. Fabricators must tweak these features
to match their process capabilities while meeting the final impedance
requirement.
Regards,
Gary Ferrari
Executive Director
IPC Designers Council
860-350-9300
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|