One of the leading manufacturers of microwave base materials is Taconic. Taconic manufactures
PTFE/woven glass base materials both in Petersburgh, NY (USA) and Mullingar (Ireland). Our web
site is www.taconic-add.com

Please call me off-site for further information

regards

Manfred Huschka
Taconic International

--- On Thu, 7 Jan 1999 17:45:43 -0700  Joe Felts <[log in to unmask]> wrote:
The most comprehensive list I've seen was QPL-13949-103 (Rev. 4-28-97) - a
worldwide listing by site - which was killed along with MIL-S-13949H.  But
there may be an equivalent replacement - check
http://www.dscc.dla.mil/Offices/Doc_Control/.

Here are a few relevant URLs:
http://www.alliedsignal.com/electronicmaterials/about/laminate/index.htm
http://www.gilam.com/
http://www.compositechltd.com/index.html
http://www.Polyclad-usa.com/mainpage.htm
http://www.norplex.com/
http://www.rogers-corp.com/mwu/
http://www.nvf.com/
http://www.synthane.com/
http://www.ge.com/electromaterials/

Joe Felts

-----Original Message-----
From:   Management Recruiters of St. Lawrence County
[SMTP:[log in to unmask]]
Sent:   Tuesday, December 22, 1998 8:17 AM
To:     [log in to unmask]
Subject:        [TN] Laminate suppliers

ok  I need some help finfing a COMPLETE list of pcb laminate suppliers to
the
pcb fabrication industry.  A subset of the suppliers of the laminate
materials used in fab of microwave type products would be especially
helpfull.

Thanks in advance,
Eric Hunt

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################



---------------End of Original Message-----------------

--------------------------------------------------------
Name: Manfred Huschka
Taconic Advanced Dielectric Division
Mullingar Business Park
Mullingar, Co. Westmeath
Republic of Ireland
Office: PF 1275, D-51676 Wipperfuerth, Germany
        Tel.: +49 2267 888004
        Fax:  +49 2267 888005
E-mail: Manfred Huschka <[log in to unmask]>
Web: http:\\www.taconic-add.com
Date: 01/08/99
Time: 09:08:19

This message was sent by Z-Mail Pro - from NetManage
NetManage - delivers Standards Based IntraNet Solutions
--------------------------------------------------------

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2