Tom,
Are you asking this just so you know the best way to run an existing board
through
the wave? Or are you trying to influence how the board is being laid out?
This first diagram shows the preferred orientation through the wave.
If you can influence the board layout, ask that they put "robber" pads on
the
trailing edge of the I. C.
Charlie B.
Tom Braswell <[log in to unmask]> on 01/11/99 03:32:43 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Tom Braswell <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Charles Barker/US/I-O INC)
Subject: [TN] Orietation of DIP IC for Solder Wave
Netters,
Someone tell me which of these two is correct for wave soldering
1. Direction thru wave -------------------->
_|__|__|__|__|__
| |
| |
|____________|
| | | | |
2. Direction thru Wave ----------------------->
_______
__| |__
__| |__
__| |__
__| |__
|_______|
Thanks,
Tom B.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|