TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Date:
Fri, 15 Jan 1999 16:44:04 -0600
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (25 lines)
Little Fuse and a couple of others. Sometimes, "German Silver" (forgot the composition but
tarnishes/oxidizes readily) is used as the case's metallic interface. Some recommendations
include (from Dr. ? at Hughes - I will get his name) using "stainless" flux. The stuff is
very active and gets the job done. Another path I took was to have the metal surface
immersion tin coated for much better solderability without the hassle but for relatively
shortened shelf life.

You seem to be on the right track from your previous position. The manual abraiding doesn't
quite get it, nor does mild flux except with different metallization. You may rund lab
analysis to determine the true case metallization.

Earl Moon

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2