Vishy: We are doing case bonding for electronic instruments. The
joint design uses tongue and groove for the bonding faces. The adhesive is a two
component methacrylate, case material is an ABS/polycarbonate. We dispense a
continous bead that includes some fairly complex radiused corners to the female
side of the case using XYZ control. The groove dimensions are not quite as tight
as yours but close.
The dispensing equipment is made by Liquid Control Corp. North Canton Ohio,
Phn#330-494-1313. I have been very satisfied with it's perfomance. Others make
similar equipment; Camelot, Sealant etc. The real key to the successful
delivery of small precision controlled amounts is the rheology of the material
you are dispensing more than the equipment.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
425-356-6076
On Fri, 8 Jan 1999 00:04:30 -0800 Narayana Vishy-CVN002 wrote:
> From: Narayana Vishy-CVN002 <[log in to unmask]>
> Date: Fri, 8 Jan 1999 00:04:30 -0800
> Subject: [TN] Adhesive/sealant applicator
> To: [log in to unmask]
>
> I am looking for a adhesive/sealant dispenser.Requirements are to precision
> dispense sealant continuosly into a 0.65 mm width groove of 05 mm depth of a
> running profile on a polycarbonate housing . Any leads ?
>
>
> Vishy.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|