Hi Roger - your question is very open ended but I'll take a stab at giving
you an answer. First, if you are just looking for basic solder alloy
information contact any of the solder alloy manufacturers (e.g. Kester,
Multicore, Indium, Alpha, Arconium, and the remaining cast of thousands) -
they will have some material properties, use environments, forms etc types
of information. Second, if you are going for more detailed information
find a copy of the following book - "Solder Mechanics: A State of the Art
Assessment", edited by Frear, Jones, Kinsman, ISBN # 0-87339-166-7. This
book isn't organized in the most user friendly manner but does contain a
host of references to the specific alloys of interest to you. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Roger Massey-G14195 <[log in to unmask]> on 01/08/99
05:50:17 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Roger Massey-G14195 <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Solder Metallurgy
Happy New Year to all "netters"
Dont know if this has been asked before, but can anybody point me
towards some metallurgical information on the standard 10Sn/88Pb/2Ag
solder alloy and its equally popular friend 95Pb/5Sn.
Any help greatly appreciated
Roger
Motorola UK
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|