The 66 asf is for a 1 amp pushed to the cell, if my memory is correct.
Use 3 amps and multiply all the ruler readings by 3, so 66 asf becomes 198
asf, which in my world is close enough.
You plating PCB's at 200+ ASF? Phew, not bad. You have aspect ratios in
the holes of 1:1?
Rudy Sedlak
RD Chemical Company
################################################################