Sheila Smith wrote:
>
> Steve, The only company I know of that sells brush plating solutions is Sifco Selective Plating in Cleveland. However a search through the Thomas Register also turned up a place call Brushtek in Chatsworth, CA. Good luck!
>
> Sheila Smith, Marconi AES
>
> ----------
> From: Leslie O. Connally
> Sent: Wednesday, January 20, 1999 9:48 AM
> To: [log in to unmask]
> Subject: Re: [TN] Assy: Source for Gold Plating Solution
>
> Hi Steve,
>
> You might try Technic, Inc. Their California rep's address is:
>
> Technic, Inc.
> 1170 Hawk Cir.
> Anaheim, Ca. 92807
> (714)632-0200
> They also have a web site at www.technic.com
>
> Another source is Lea-Ronal. The only address I have is a New York address, but
> I'm sure they must have a West coast rep. Their address is:
>
> Lea Ronal
> 272 Buffalo Avenue
> Freeport, N.Y. 11520
> (516)868-8800
>
> Their President is Richard Kessler.
> > From: "Stephen R. Gregory" <[log in to unmask]>, on 1/19/99 1:57 PM:
> > Hello out there!
> >
> > Remember my post last week about solder preforms for PC104 connectors?
> > Remember what I was whining about? 'Bout the difficulty in hand soldering
> > those things without getting solder on the gold plating?
> >
> > Well, you can guess what this email is about...I need some gold plating
> > solution now. (BIG surprise there huh?)
> >
> > The source I used to get it from here in "Silicon Valley" has
> > disappeared...does anybody know of another source I can buy it from? It
> > would
> > be kinda' nice if it was here in the valley, but not nessesary.
> >
> > I'd sure appreciate it!
> >
> > -Steve Gregory-
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with following
> > text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> > for additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> > 847-509-9700 ext.312
> > ################################################################
> >
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
Steve: Try
CIRCUIT TECHNOLOGY CENTER 45 Research Drive, Haverhill, MA, 01832-1293
USA 978.374.5000 Fax 372.5700 [log in to unmask] www.circuitnet.com
TTYL
Dave F
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|