In going back and thinking about this (since I sometimes like to connect two
"radiating" areas of copper on opposite sides of the board with vias for
heat conduction), I wondered: solder is not a great heat conductor, but it
is better than air or solder mask, isn't it? What do you think would be a
good way to achieve a "thermal via"?
Seth Goodman
Goodman & Associates
7687 Leta Way
Verona, WI 53593
Tel (608)833-9933
Fax (608)833-9966
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
> Sent: Thursday, December 17, 1998 4:25 PM
> To: [log in to unmask]
> Subject: [TN] FAB: Solder Filled Thermal Vias
>
>
> I may be wrong interpreting your question, but it seems you want
> to get heat out. Are these vias
> "heat pipes?" If so, keep them open. As you know, solder is not a
> good thermal conductor.
>
> Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask]
> or 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|