Richard ,
There are lot of people like us , still using tin-lead as etch resist . Very
rarely we are re-flowing tin/lead .
Why we are still working with tin/lead instead of pure tin ? Mainly due to
inertion . The process is working , we do not have environmental problems
with lead ( there is enough sulfates to settle it ) . Tin as etch resist is
not considerable cheaper compared to tin/lead . Not smart answer , but real
one .
At 11:23 06/01/99 EST, you wrote:
>for my own curiosity - how many people are still using a tin/lead bath for
>plating tin/lead ( other than maybe a military spec ) and why?
>
>response would be greatly appreciated
>
>Richard Fudalewski
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
Edward Szpruch
Eltek Ltd - Israel
e-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|