This is a fairly in depth subject however the main causes of warp are usually
design related in terms of the internal construction of the board being a
balanced layout. Bonded heatsinks also tend to cause an imbalance. When
dissimilar materials are joined and subjected to heat processes they expand and
contract at differing rates resulting in deviation from flatness. It would
worry me if your supplier is "flattening" these boards since they will tend to
retain a "memory" of the initial warp and your reflow process is relieving
stresses and this explains why they are warping.
In summary, the root cause is probably board design however there are other
possibilities such as base laminate quality which, although rarer in occurence,
can cause the same problem.
Regards
Bryan Kerr
Alenia Marconi (Scotland)
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|