TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
KELLY M SCHRIVER <[log in to unmask]>
Date:
Fri, 22 Jan 1999 15:40:00 -0500
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, KELLY M SCHRIVER <[log in to unmask]>
Parts/Attachments:
text/plain (24 lines)
Good afternoon Donn

Bare boards are normally tested prior to application of organic coatings, to
avoid the affects of test probe punctures in the coat during storage and
processing.

By the time one has assembled and soldered the circuit card assembly to the
point of being ready for in circuit test, the organic coat has either been
displaced by the solder application or removed by cleaning process.

Regards - Kelly

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2